Electrical Properties Metric English Comments
Dielectric Strength 12.8 - 17.0 kV/mm
325 - 432 kV/in
Average value: 14.0 kV/mm Grade Count:13
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
Dielectric Strength 14.0 - 17.0 kV/mm
356 - 432 kV/in
Average value: 15.2 kV/mm Grade Count:12
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..