Polymer Property : Dielectric Strength = 17.1 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 17.1 kV/mm
434 kV/in
60Hz, Short Time, dry; ASTM D149
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group
Dielectric Strength 17.1 kV/mm
435 kV/in
Master Bond EP46HT Epoxy Adhesive for Structural Bonding
Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f..
Dielectric Strength 17.1 kV/mm
435 kV/in
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F
Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°..
Dielectric Strength 17.1 kV/mm

@Thickness 3.17 mm
435 kV/in

@Thickness 0.125 in
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System
Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr..
Dielectric Strength 17.1 kV/mm
435 kV/in
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive
TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre..
Dielectric Strength 17.1 kV/mm
434 kV/in
Short Time; ASTM D149
Plenco 6500 Phenolic, Briquette, Transfer Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..
Dielectric Strength 17.1 kV/mm
435 kV/in
ASTM D149
3M Scotchcast™ 3570G-N Connector Sealing Pack
The 3M Scotchcast Connector Sealing Pack 3570G-N insulates and provides protection for electrical spring connectors against dust, soil, water, and other environmental elements. Each sealing pack con..
Dielectric Strength 17.1 kV/mm
434 kV/in
Dow Corning 3110 SILICONE RUBBER ENCAPSULANT
Two-part, white, condensation cure, moderate flow, general purpose encapsulant, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning
Dielectric Strength 17.1 kV/mm
434 kV/in
Wet, short term. ASTM D149
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI..