Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.1 - 19.7 kV/mm | 460 - 500 kV/in | Average value: 19.5 kV/mm Grade Count:18 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS 484 GY Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS LE BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 8813148Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS WT Availability: North AmericaForms: PelletsAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 AF Colors Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricateAppearance: Colors AvailableInformation provi.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 E HS N Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Nucleating AgentFeatures: Heat Stabilized and NucleatedProcessing Method: ExtrusionTPCI# 9587102Information provided by TP Comp.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 E2 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 L LE MB Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low ExtractablesAppearance: Colors AvailableTPCI# 7964102Information provide.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 X BN071 EL MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Fast Molding Cycle, Good Processability, Lubricated and NucleatedTPCI# 1033102Information provided by TP Co.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6 E M/SL4 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant and Silicone LubricantFeatures: Low Friction, Good Wear Resistance and LubricatedAppearance: BlackInformation provid.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 IM 6040 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 L N Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Copolymer, Fast Molding Cycle, Nucleated and LubricatedProcessing Method: Injection MoldingInformation prov.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS TM10 WT155 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | |
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive TRA-BOND 2143D is a medium viscosity adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are required. This tw.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | |
Aremco Aremco-Bond™ 2150 High Performance Epoxide Ceramic-Filled, Fast-Setting, High Vibration Resistance and Bond Strength. Ideal for bonding ceramic wear tiles. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | |
Atom Adhesives AA-BOND FS227 Epoxy Adhesive AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | ASTM D149 |
Arlon R38726R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeThis data represents typical values for the production material. The.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PBT FR-C Availability: North AmericaForms: PelletsFeatures: Flame RetardantUL File Number: E157318Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |