Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.0 kV/mm | 635 kV/in | STN EN 60243-2 |
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Nylacast Impact Nylon 6, Impact Grade Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Permabond 735 Cyanoacrylate, toughened PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Permabond 801 Cyanoacrylate, High Temperature PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 1.00 mm |
635 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | Average value: 29.2 kV/mm Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Global EPP PA 6E Extruded Polyamide 6 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Shin-Etsu Silicones KE-3472T Silicone, RTV Conformal Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 1.60 mm |
635 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 1.60 mm |
635 kV/in @Thickness 0.0630 in |
in air; ASTM D149 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses). |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243 |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 2.00 mm |
635 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo Vylopet® EMC245K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® F136-DH Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | cond; IEC 60243-1 |
DSM Akulon® K224-G6-FC NA99001 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K225-KWS (Cond.) Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | cond; IEC 60243-1 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Covestro Bayblend® KU 2-1468 Polycarbonate/ABS Blend Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Dielectric Strength | 25.0 - 30.0 kV/mm | 635 - 762 kV/in | ASTM D149 |
Adamas Adalon® 413 PTFE, 20% PPS Information provided by Adamas, HPM |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® S240-C Nylon 66 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Ineos ABS NOVODUR® P2T ABS, Injection Grade
(discontinued **) Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g.. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 1.00 mm |
635 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |