Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.3 kV/mm | 262 kV/in | Short Term per ASTM D149. |
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p.. |
|||
Dielectric Strength | 10.3 kV/mm | 262 kV/in | Step by Step; ASTM D149 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Dielectric Strength | 10.3 kV/mm | 262 kV/in | Step by Step; ASTM D149 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Dielectric Strength | 10.3 kV/mm | 262 kV/in | Step by Step; ASTM D149 |
Plenco 3557 Phenolic, Granular, Compression Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |
|||
Dielectric Strength | 10.3 kV/mm | 262 kV/in | Short Time; ASTM D149 |
Plenco 3557 Phenolic, Granular, Transfer Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |