Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.00 - 10.5 kV/mm @Temperature 90.0 °C |
203 - 267 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Dielectric Strength | 8.00 - 10.5 kV/mm @Temperature 90.0 °C |
203 - 267 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |