Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Dielectric Strength | 27.6 - 100 kV/mm | 701 - 2540 kV/in | Average value: 54.8 kV/mm Grade Count:49 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | DC; ASTM D149 |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Dielectric Strength | 27.6 kV/mm @Thickness 1.60 mm |
701 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF30 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedUL File Number: E157318Appearance: Bla.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF33 L N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: Fast Molding Cycle and LubricatedAppearance: BlackTPCI# 87.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D-149 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.062" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Dielectric Strength | 27.6 kV/mm | 701 kV/in | 1" electrode in air; ASTM D149 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Dielectric Strength | >= 27.6 kV/mm | >= 700 kV/in | At 20 mils; ASTM D3755 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | In Oil; ASTM D149 |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51146R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
Dielectric Strength | 27.6 kV/mm | 701 kV/in | Arlon- SQA-TMS-020 |
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51106R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Dielectric Strength | 27.6 kV/mm | 702 kV/in | Arlon- SQA-TMS-020 |
Arlon 920-10B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
3M EPS-400 Heat Shrink Tubing 3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon R37881R015 Silicone Rubber/Fiberglass Interleave: 1.5 mil PE; Side 1: uncured silicone rubber; Substrate: 1528 fiberglass; Side 2: uncured silicone rubber; Interleave: 1.5 mil PE |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF5 HS 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, .. |