Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 65.0 - 146 kV/mm | 1650 - 3710 kV/in | Average value: 75.1 kV/mm Grade Count:8 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |