Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 40.2 kV/mm @Thickness 1.00 mm |
1020 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Dielectric Strength | 40.2 kV/mm @Thickness 1.00 mm |
1020 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Dielectric Strength | 40.2 kV/mm | 1020 kV/in | ASTM D149 |
Unitika L-8005 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Dielectric Strength | 40.2 kV/mm | 1020 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |