Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific) CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY5210 PC+ABS (Europe-Africa-Middle East) CYCOLOY CY5210 is a flame retardant PC/ABS using non-chlorinated and non-brominated FR additives for injection moulding. CYCOLOY CY5210 has an improved hydrolytic stability with balanced flow and im.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East) GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 101 PC (Europe-Africa-Middle East) LEXAN 101 is a high viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 104R PC (Europe-Africa-Middle East) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility informat.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 915R PC (Europe-Africa-Middle East) Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 923A PC (Europe-Africa-Middle East) LEXAN 923A is a medium viscosity flame retardant grade, UV-stabilized, especially suitable for electrical applications. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® EXL6033 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with good processability.Very low temp. ductility, UV-Stabilized, UL94 V1 rated in white colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® LUX2180T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2180T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | Conditioned; ASTM D149 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | Short Time; ASTM D149 |
Plenco 51240 PET, Pellet, Injection Molded, Green
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® ML3732 PC (Europe-Africa-Middle East) Lexan ML3732 is a low viscosity flame retardant grade, especially designed to pass the glow wire test according EDF HN60-S-02 at a thickness of 3.2 mm. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | 70°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1301EP22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | IEC 60243-1 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Dielectric Strength | >= 17.0 kV/mm | >= 432 kV/in | |
Arlon 0.011" (0.2794 mm) Uncured Silicone Traction Motor Insulation (P29600R011) 0.006 in., +0.002, -0.001(0.2 mm, +0.05, -0.03) uncured silicone on 0.005 in. (0.08 mm) nominal PTFE coated fiberglass; 0.0015 in. (0.038 mm) polyethylene interleave; overall thickness 0.011 in ±0... |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 953A PC (Europe-Africa-Middle East) LEXAN 953A is a high viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |