Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 45.75 kV/mm | >= 1162 kV/in | ASTM D149 |
Arlon 31140R025 0.032" Uncured Silicone Rubber on Release Coated HDPE Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberRelease Carrier: Release Coated HDPEThis data represents typical values for the production material and should no.. |
|||
Dielectric Strength | 45.75 kV/mm | 1162 kV/in | ASTM D149 |