Electrical Properties Metric English Comments
Dielectric Strength 181 kV/mm
4600 kV/in
Von Roll Isola IMI Varnish 709 Solventless Polyester Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 76°C. Usag..
Dielectric Strength 181 kV/mm

@Thickness 0.102 mm
4600 kV/in

@Thickness 0.00400 in
ASTM D149
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin
High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera..