Electrical Properties Metric English Comments
Dielectric Strength 16.0 - 19.0 kV/mm

@Thickness 0.100 mm
406 - 483 kV/in

@Thickness 0.00394 in
short term; ASTM D149
Polikim EFALON® C-15 PTFE, 15% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
Dielectric Strength 13.0 - 19.0 kV/mm
330 - 483 kV/in
ASTM D149
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Dielectric Strength 13.0 - 19.0 kV/mm
330 - 483 kV/in
ASTM D149
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Dielectric Strength 14.0 - 19.0 kV/mm
356 - 483 kV/in
Average value: 15.7 kV/mm Grade Count:10
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Dielectric Strength 16.0 - 19.0 kV/mm
406 - 483 kV/in
ASTM D149
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Dielectric Strength 16.0 - 19.0 kV/mm
406 - 483 kV/in
ASTM D149
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Dielectric Strength 16.9 - 19.0 kV/mm
430 - 483 kV/in
Average value: 17.8 kV/mm Grade Count:7