Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.0 - 21.0 kV/mm | 432 - 533 kV/in | Average value: 18.8 kV/mm Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Dielectric Strength | 14.0 - 21.0 kV/mm | 356 - 533 kV/in | Average value: 16.5 kV/mm Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |