Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 57.1 kV/mm | 1450 kV/in | IPC TM-650 2.5.6.2 |
Arlon 85N Polyimide Laminate and Prepreg 85N is a polyimide and laminate prepreg system for PWBs requiring resistance to high temperature, both in process and in end-use application. Bromine-free chemistry provides thermal stability for a.. |