Polymer Property : Dielectric Strength = 583 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 23.0 kV/mm
583 kV/in
Saint-Gobain CHR® 23816 Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape
Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal ..
Dielectric Strength 23.0 kV/mm
583 kV/in
ASTM D149
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep..