Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 3.17 mm |
610 kV/in @Thickness 0.125 in |
ASTM D149 |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® KU 2-1473 Polycarbonate/ABS Blend
(discontinued **) Matter surfaces than standard grades; injection molding.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new nam.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D-149 |
Chevron Phillips Xtel® XE3200NA Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XE3200NA is an un-reinforced high performance, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information provided b.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Butyl Rubber (IIR, CIIR, BIIR) Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and ca.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
ASTM D149 |
Manifattura Cattaneo PEEK Polyetheretherketone Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.00 mm |
610 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243 |
Solvay TECHNYL® B 216 Natural D PA66/6, Conditioned Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.60 mm |
610 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 2410R PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | Oil(Molding); ASTM D149 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Polyplastics FR-PET® C3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60250 |
Polyram RamLloy PBB704 PC/ABS Alloy, UV Stabilized PC/ABS alloy, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Polyplastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® T 44 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 45 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® T 65 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.00 mm |
610 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 992 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
ASTM D149 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | VDE 0303/4 |
Polyram RamTal PM1009 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |