Polymer Property : Dielectric Strength = 63.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
Quantum PVDF
Information provided by Quantum Advanced Engineering Plastics
Dielectric Strength 63.0 kV/mm
1600 kV/in
Short Term; 10 mil film; ASTM D149
ScanTube PVDF Tubing
Information provided by ScanTube, Inc.
Dielectric Strength 63.0 kV/mm
1600 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Dielectric Strength 63.0 kV/mm
1600 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Dielectric Strength 63.0 kV/mm
1600 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Dielectric Strength 63.0 kV/mm
1600 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Dielectric Strength 63.0 kV/mm
1600 kV/in
50 V/sec; ASTM D149
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade)
Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a..
Dielectric Strength 63.0 kV/mm
1600 kV/in
IPC TM-650 2.5.6.2
Arlon 38N High Performance Polyimide Low-Flow
38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow..
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
3M 7959MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
3M 9059MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..