Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 - 26.0 kV/mm | 400 - 660 kV/in | Average value: 18.5 kV/mm Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Dielectric Strength | 14.0 - 26.0 kV/mm | 356 - 660 kV/in | DIN 53481 |
Isoflon PUR Polyurethane Very high wear resistanceHighly resilientInformation provided by Isoflon. |
|||
Dielectric Strength | 16.0 - 26.0 kV/mm | 406 - 660 kV/in | Average value: 19.8 kV/mm Grade Count:9 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |