Electrical Properties Metric English Comments
Dielectric Strength 29.5 kV/mm
750 kV/in
Cured
Resin Technology Group UV-406 High Clarity, Moisture Resistant, UV Curing Bonder
UV 406 is a rapidly curing UV adhesive developed for use in bonding a variety of plastics, glass and metals, where moisture resistance and low shrinkage during cure is critical. Bond strengths on po..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)<
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be ..
Dielectric Strength 29.5 kV/mm
750 kV/in
Saint-Gobain CHR® SG03-03(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Strength 29.5 kV/mm
750 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Plastiblend® ABS/PBT 1500
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Dielectric Strength 29.5 kV/mm
750 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Plastiblend® PBT/ABS BK
Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc.
Dielectric Strength 29.5 kV/mm

@Thickness 1.59 mm,
Temperature 25.0 °C
750 kV/in

@Thickness 0.0625 in,
Temperature 77.0 °F
Cytec EN-9 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Dielectric Strength 29.5 kV/mm
750 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 920-10R##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape
1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 920-10T##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Transparent, Rectangular cross-section, S..
Dielectric Strength 29.5 kV/mm
750 kV/in
Arlon SQA-TMS-020
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum ..
Dielectric Strength 29.5 kV/mm
750 kV/in
Original; ASTM D4325
3M Scotch™ 130C Linerless Rubber Splicing Tape
3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice..
Dielectric Strength 29.5 kV/mm
750 kV/in
24 hrs in water; ASTM D4325
3M Scotch™ 130C Linerless Rubber Splicing Tape
3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
Dielectric Strength 29.5 kV/mm
750 kV/in
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat
Approved to GMP.PP.013
Dielectric Strength >= 29.5 kV/mm
>= 750 kV/in
IPC TM-650 2.5.6.2
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg
45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 51100R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT..
Dielectric Strength <= 29.5 kV/mm
<= 750 kV/in
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled
Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C)
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 29.5 kV/mm
750 kV/in
ASTM D149
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b..
Dielectric Strength >= 29.5 kV/mm
>= 750 kV/in
ASTM D149
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use..
Dielectric Strength 29.5 kV/mm
750 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 29.5 kV/mm
750 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..