Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 40.0 - 80.0 kV/mm @Thickness 0.100 mm |
1020 - 2030 kV/in @Thickness 0.00394 in |
short term; ASTM D149 |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | ASTM D149; ISO.243 DN.53481 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | ASTM D149; ISO.243 DN.53481 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Dielectric Strength | 19.7 - 80.0 kV/mm | 500 - 2030 kV/in | Average value: 36.3 kV/mm Grade Count:9 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 19.7 - 80.0 kV/mm | 500 - 2030 kV/in | Average value: 33.5 kV/mm Grade Count:11 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Dielectric Strength | 15.7 - 80.0 kV/mm | 400 - 2030 kV/in | Average value: 33.2 kV/mm Grade Count:35 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Dielectric Strength | 15.0 - 80.0 kV/mm | 380 - 2030 kV/in | Average value: 28.9 kV/mm Grade Count:46 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm @Thickness 0.200 mm |
1270 - 2030 kV/in @Thickness 0.00787 in |
VDE 0303 Part 2 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | DIN 53481 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | DIN 53481 |
Isoflon FEP Fluorinated Ethylene Propylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | DIN 53481 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 40.0 - 80.0 kV/mm | 1020 - 2030 kV/in | DIN 53481 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Dielectric Strength | 40.0 - 80.0 kV/mm | 1020 - 2030 kV/in | DIN 53481 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 60.0 - 80.0 kV/mm | 1520 - 2030 kV/in | Air (Tape); ASTM D149 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Dielectric Strength | 60.0 - 80.0 kV/mm | 1520 - 2030 kV/in | Air (Tape); ASTM D149 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Dielectric Strength | 60.0 - 80.0 kV/mm | 1520 - 2030 kV/in | ASTM D149 |
Adamas Adalon® 992 Modified PTFE Information provided by Adamas, HPM |
|||
Dielectric Strength | 15.4 - 80.0 kV/mm | 390 - 2030 kV/in | Average value: 20.4 kV/mm Grade Count:137 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Dielectric Strength | 11.0 - 80.0 kV/mm | 280 - 2030 kV/in | Average value: 23.9 kV/mm Grade Count:27 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |