Electrical Properties Metric English Comments
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 M350 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 P250 EPY Pelletized Carbon Fiber, Epoxy Sizing
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 P350 GLY Pelletized Carbon Fiber, Glycerine Sizing
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 P350 PUT Pelletized Carbon Fiber, Polyurethane Sizing
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S001 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S003 APS Staple Carbon Fiber, Aromatic Polymer Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S003 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S003 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S006 APS Staple Carbon Fiber, Aromatic Polymer Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S006 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S006 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S006 PUT Staple Carbon Fiber, Polyurethane Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S009 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S009 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S012 EPY Staple Carbon Fiber, Epoxy Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 S012 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 M100 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
SGL Carbon Group SIGRAFIL C® C25 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
cured 24 hrs @ 25°C
Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive
TRA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled ..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
cured 24 hrs @ 25°C
Atom Adhesives AA-DUCT 2919 Epoxy Adhesive
AA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require good flexibility coupled w..
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
Cured: 24 hours at 25°C
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit..