Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 M350 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 P250 EPY Pelletized Carbon Fiber, Epoxy Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 P350 GLY Pelletized Carbon Fiber, Glycerine Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 P350 PUT Pelletized Carbon Fiber, Polyurethane Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S001 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S003 APS Staple Carbon Fiber, Aromatic Polymer Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S003 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S003 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S006 APS Staple Carbon Fiber, Aromatic Polymer Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S006 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S006 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S006 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S009 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S009 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S012 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 S012 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 M100 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C25 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | cured 24 hrs @ 25°C |
Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive TRA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled .. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | cured 24 hrs @ 25°C |
Atom Adhesives AA-DUCT 2919 Epoxy Adhesive AA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require good flexibility coupled w.. |
|||
Volume Resistivity | 0.0016 ohm-cm | 0.0016 ohm-cm | Cured: 24 hours at 25°C |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |