Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PEI 04008 MB Availability: North AmericaForms: PelletsFeatures: Conductive and CopolymerInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 1030 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS 03011 BK MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Appearance: BlackIn.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
Techmer ES Electrablend® HDPE C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackTPCI# 9411115Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6 04001 FR MB Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequen.. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0365 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0425 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | IEC 60093 |
Teijin Panlite® BS-8110R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Volume Resistivity | <= 1.0 ohm-cm | <= 1.0 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **) PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te.. |