Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | STN IEC 60093 |
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® 134 PC Nonhalogenated. 3.5 MFR. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 223 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 943A PC Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig.. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 141 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | Conditioned; IEC 60093 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 AF Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedInformat.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PPS GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | D257 |
Zhejiang Juner PC-A6-2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm @Temperature 23.0 °C |
1.00e+17 ohm-cm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm @Temperature 25.0 °C |
1.00e+17 ohm-cm @Temperature 77.0 °F |
100 V DC 50% RH 1000 sec electrification time; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm @Temperature 25.0 °C, Time 100 sec |
1.00e+17 ohm-cm @Temperature 77.0 °F, Time 0.0278 hour |
100 V DC; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 75 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | IEC 60093 |
Arkema Group Pebax® MH 2030 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MH 2030 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 2030 is an inherently dissipative polymer and can be dry blended or compounded w.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM-D257 |
Braskem PCD 0140 HECO Polypropylene Heterophasic Copolymer PCD 0140 is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140 is highly protected against thermal aging and.. |
|||
Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film Rogers 3001 bonding film is a thermoplastic chloro-fluorocopolymer. It is recommended for bonding low dielectric constant PTFE (Teflon® fluorocarbon polymer) microwave stripline packages and other.. |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |
|||
Volume Resistivity | >= 1.00e+17 ohm-cm @Temperature 20.0 °C |
>= 1.00e+17 ohm-cm @Temperature 68.0 °F |
|
Advanced Ceramics ACL 1091 (C-799) Alumina Information provided by Advanced Ceramics Limited (ACL) |