Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PP 1395 PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East) LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin.. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF10 A1 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® POM CO Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and Medium ViscosityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX99620C PC LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EE005E PEI LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 LGCF50 HS BK 6mm 50% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAp.. |
|||
Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific) LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 03005 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
Techmer ES HiFill® PPS 0334 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Lennite® CN-P UHMW Polyethylene (conductive) Carbon-powder-filled, self-lubricating, conductive material with excellent abrasion-resistance and high impact strength. This material is light weight and easily machined, has good chemical and str.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive) Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an exc.. |
|||
Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Volume Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Verton OX07411 PPS LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |