Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data) Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data) This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Volume Resistivity | 1.0e+14 - 1.0e+16 ohm-cm | 1.0e+14 - 1.0e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Volume Resistivity | 1.0e+14 - 1.0e+16 ohm-cm | 1.0e+14 - 1.0e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Volume Resistivity | 1.0e+14 ohm-cm | 1.0e+14 ohm-cm | ASTM D257 |
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM) Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |