Polymer Property : Volume Resistivity = 2.00e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
Z direction; C96/35/90; ASTM D257
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Permabond TA436 Toughened Acrylic Adhesive
PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Permabond TA4810 Toughened Acrylic Adhesive
PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites.  TA4810 has excellent adhesion to as received metal surfac..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Permabond TA4246 Toughened Acrylic Adhesive
PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with ..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
60°C for 500 hrs with 90% RH; JIS-K-6249
Fujipoly Industries Sarcon® GR-b Gap Filler Pad
Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
60°C for 500 hrs with 90% RH; JIS-K-6249
Fujipoly Industries Sarcon® GR-Hb Gap Filler Pad
Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 GF33 IM L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 IM 40 Z
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 IM 407 L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 IM 409 L MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 IM 435 HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6 IM HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Plastiblend® PA6/ABS 1120 B1
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc.
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
IEC 60093
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, Conditioned
Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent ..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6/ABS 1120 B1
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Techmer ES HiFill FR® PA6 FR-N IM
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated Appearance: ..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D247
Plenco 3356 Phenolic, Granular, Compression Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Toyobo PELPRENE™ S2001 Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Volume Resistivity >= 2.00e+13 ohm-cm
>= 2.00e+13 ohm-cm
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy
Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan..