Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | |
Pyrotek TS-82 Thermoset Electrical Insulation Product (Nema Grade: XXX) Paper reinforcement, Phenolic Resin, Natural Color. High humidity resistance, Excellent resistance to splitting.Information provided by Pyrotek. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | |
XXX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | 125°C for 1,000 hrs; JIS-K-6249; ASTM D257 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Volume Resistivity | >= 3.00e+13 ohm-cm | >= 3.00e+13 ohm-cm | ASTM D 257 |
Karina E 890-25/1-CR-IS Natural PVC Compound Flame retardant and oil resistant PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°C.Information provided .. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | ASTM D247 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika A1030BRL PA6, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika A1030FR PA6, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika A1030SR PA6, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika EX-1222 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika A1030JR PA6, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika A1030TF PA6, Dry Lubricating nylonInformation provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Unitika EX-1030 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
Polyplastics Duracon® SF-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
DSM Arnite® AV2 370 XL-T PET-GF35 35% Glass Reinforced, Low Outgassing, Thermal conductive material |
|||
Volume Resistivity | <= 3.00e+13 ohm-cm | <= 3.00e+13 ohm-cm | |
Cytec (Conap) RN-1210 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | >= 3.00e+13 ohm-cm | >= 3.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 301-1 Optical Grade Epoxy Material Description: A two component, room temperature curing, optical grade epoxy, designed for optics, medical, and opto-electronic packaging of semiconductor devices, components, and electronics.. |
|||
Volume Resistivity | >= 3.00e+13 ohm-cm | >= 3.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti.. |
|||
Volume Resistivity | <= 3.00e+13 ohm-cm | <= 3.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy Product Description: EPO-TEK® 509FM-1 is a two component, optically opaque epoxy designed for potting of semiconductors, PCB and systems-level electronics. It can be used in many electronic indust.. |
|||
Volume Resistivity | <= 3.00e+13 ohm-cm | <= 3.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 730 General Purpose Epoxy Product Description: EPO-TEK® 730 is a two component, thixotropic, room temperature-curing epoxy adhesive. Advantages & Application Notes: Excellent all purpose adhesive. Many uses in job shop and .. |
|||
Volume Resistivity | >= 3.00e+13 ohm-cm | >= 3.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® U300-2 Two Component Epoxy Material Description: A two component epoxy designed for capillary underfill of semiconductor chips and SMDs. Long potlife, high Tg, and optical clarity are a few of its traits. NASA approved lo.. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | |
Abatron AboCast 8103-28 High-Performance Dielectric Epoxy AboCast 8103-28 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |
|||
Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | |
Aremco Aremco-Bond™ 2310 High Performance Epoxide Ceramic-Filled, 1:1, High Lap Shear and Peel Strength, Autoclavable. |
|||
Volume Resistivity | 3.00e+13 ohm-cm @Temperature 23.0 °C |
3.00e+13 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 92 Flexible PVC, Flame Retardant Insulation General purposes |