Polymer Property : Volume Resistivity = 3.16e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 - 3.16e+11 ohm-cm
1.00e+11 - 3.16e+11 ohm-cm
IS 3396-1979
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow ..
Volume Resistivity 3.16e+10 - 3.16e+11 ohm-cm
3.16e+10 - 3.16e+11 ohm-cm
IS 3396-1979
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec..
Volume Resistivity 1.00e+11 - 3.16e+11 ohm-cm
1.00e+11 - 3.16e+11 ohm-cm
IS 3396-1979
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche..
Volume Resistivity 1.00e+11 - 3.16e+11 ohm-cm
1.00e+11 - 3.16e+11 ohm-cm
IS 3396-1979
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric ..
Volume Resistivity 1.00e+11 - 3.16e+11 ohm-cm
1.00e+11 - 3.16e+11 ohm-cm
IS 3396-1979
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni..
Volume Resistivity 1.00e+11 - 3.16e+11 ohm-cm
1.00e+11 - 3.16e+11 ohm-cm
IS 3396-1979
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication ..