Electrical Properties Metric English Comments
Volume Resistivity 5.01e+10 ohm-cm
5.01e+10 ohm-cm
ASTM D257
Tipco Tipcolite® TX 211 Phenolic Compound, Wood Flour, having Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Switchgear, HRC FusesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.