Eurotec > Polyethylene Terephthalate (PET)
Manufacturer :
Eurotec
>
Category :
Polyethylene Terephthalate (PET)
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
Eurotec® Tecodur® PB70 GR15 NL100 KA01 PBT/PET, 15% glass fiber reinforced, heat stabilized, natural, gas injection grade
Polybutylene Terephthalate (PBT), Heat Resistant
Tecodur®
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural
PBT + PET Blend, Glass Filled
Tecodur®
Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced
Polybutylene Terephthalate (PBT)
Tecodur®
Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0
Polybutylene Terephthalate (PBT)
Tecodur®
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural
Polybutylene Terephthalate (PBT), Heat Resistant
Tecodur®
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural
Polybutylene Terephthalate (PBT), Heat Resistant
Tecodur®
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced
Polybutylene Terephthalate (PBT)
Tecodur®
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural
Polybutylene Terephthalate (PBT), Heat Resistant
Tecodur®
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural
Polybutylene Terephthalate (PBT), Heat Resistant
Tecodur®
Eurotec® Tecopet® PT70 GR15 NL100 MB PET, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR30 NL100 PR PET, 30% glass fiber reinforced, high heat stabilized, natural, fast crystallization grade
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 GR45 NL100 PR PET, 45% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Polyethylene Terephthalate (PET), 50% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Tecopet®
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade
PET + Carbon Fiber
Tecopet®
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade
PET + Carbon Fiber
Tecopet®
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT74 GR30 NL XA60 PET, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free,, heat stabilized, natural
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Tecopet®
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black
Polyethylene Terephthalate (PET), 50% Glass Reinforced
Tecopet®