PRODUCT NO. Category Trade Name
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66 Nylon 66, 40% Glass Fiber Filled Kopa®
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66 Nylon 66, 40% Glass Fiber Filled Kopa®