PRODUCT NO. Category Trade Name
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 680 Fiberglass and Glass Reinforced Phenolic Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac Phenolic, Novolac, Glass Filled
Sumitomo Bakelite North America RX® 865M Novolac Phenolic Phenolic, Novolac, Glass Filled