Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa

Category Other Engineering Material , Composite Core Material , Wood and Natural Products , Wood , Hardwood
Manufacturer 3A Composites Core Materials
Trade Name BALTEK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent bond with all types of resins and adhesives. It is compatible with a variety of manufacturing processes and is resistant to temperature changes, or exposure to fire, or chemicals such as styrene. BALTEK SB is an ideal core material for an extensive range of applications. All while being a renewable resource.Characteristics: Extremely high strength and stiffness to weight ratiosExcellent fire performanceEcological productWide operating temperature range -212 °C to +163 ° C (-414 °F to +325 °F)Excellent fatigue resistanceGood sound and thermal insulationHigh impact strengthGood moisture resistanceApplicationsMarine: Hulls, decks, bulkheads, superstructures, interiors, tooling + moldsRoad and Rail: Floors, walls, roof panels, body panels, interiors, front-ends, side skirtsWind Energy: Rotor blades, spinners, nacelle covers, generator housingsAircraft: Floor panels, galley carts, interior partitions, cargo pallets, containers, general aviation (sport aircraft) partsDefense: Naval vessels, containers, cargo pallets, sheltersIndustrial: Tooling, tanks, ductwork, impact limiter, concrete forms, fascia panels, skis, snowboards, wakeboards
Physical Properties Metric English Comments
Density 0.0940 g/cc
0.00340 lb/in³
apparent nominal; ASTM C271
Mechanical Properties Metric English Comments
Tensile Strength 7.40 MPa
1070 psi
perpendicular to plane; ASTM C297
Tensile Modulus 2.20 GPa
319 ksi
perpendicular to plane; ASTM C297
Compressive Strength 6.30 MPa
914 psi
perpendicular to plane; ASTM C365
Compressive Modulus 1.993 GPa
289.1 ksi
perpendicular to plane; ASTM C365
Shear Modulus 0.106 GPa
15.4 ksi
ASTM C273
Shear Strength 1.80 MPa
261 psi
ASTM C273
Thermal Properties Metric English Comments
Thermal Conductivity 0.0480 W/m-K
0.333 BTU-in/hr-ft²-°F
ASTM C177
Users viewing this material also viewed the following: