Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3D Systems Accura® 50 Plastic for SLA® Systems

Category Polymer , Rapid Prototyping Polymer
Manufacturer 3D Systems Corporation
Trade Name Accura®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3D Systems Accura® 50 Plastic for SLA® Systems.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and test for many uses, including:Enclosures, covers and cases for consumer goodsToysCellular/mobile telephonesElectronic components: connectors, interconnects, routing enclosures, etc.Automotive design elements: dash boards, air conditioning vents, etc.Accurate, durable master patterns for RTV or silicone moldingLimited snap-fits and assembliesSimulate a molded partConcept modelsMarketing modelsAll information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.14 g/cc

@Temperature 25.0 °C
0.0412 lb/in³

@Temperature 77.0 °F
Liquid
1.21 g/cc

@Temperature 25.0 °C
0.0437 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 600 cP

@Temperature 30.0 °C
600 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Tensile Strength, Yield 48.0 - 50.0 MPa
6960 - 7250 psi
ASTM D638
Elongation at Break 5.3 - 15 %
5.3 - 15 %
ASTM D638
Tensile Modulus 2.48 - 2.69 GPa
360 - 390 ksi
ASTM D638
Flexural Strength 72.0 - 77.0 MPa
10400 - 11200 psi
ASTM D790
Flexural Modulus 2.21 - 2.34 GPa
321 - 339 ksi
ASTM D790
Izod Impact, Notched 0.165 - 0.281 J/cm
0.309 - 0.526 ft-lb/in
ASTM D256
Penetration 4.5
4.5
mils
Thermal Properties Metric English Comments
CTE, linear 73.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
40.6 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
164 µm/m-°C

@Temperature 90.0 - 150 °C
91.1 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 53.0 °C
120 - 127 °F
ASTM D648
74.0 - 80.0 °C
165 - 176 °F
with 160ºC thermal postcure; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 - 46.0 °C
109 - 115 °F
ASTM D648
Glass Transition Temp, Tg 62.0 °C
144 °F
DMA, E"
Descriptive Properties Value Comments
Appearance Opaque natural or opaque grey
Critical Exposure (mJ/cm²) 9
Tested Build Styles FAST™, EXACT™, Exact HR
Copyright © lookpolymers.com All Rights Reserved