Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3D Systems Accura® 55 Plastic for SLA® Systems

Category Polymer , Rapid Prototyping Polymer
Manufacturer 3D Systems Corporation
Trade Name Accura®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3D Systems Accura® 55 Plastic for SLA® Systems.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic componentsTesting of functional assembliesRigid and durable functional prototypesConcept and marketing modelsAccurate, durable master patterns for urethane castingAll information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.13 g/cc

@Temperature 25.0 °C
0.0408 lb/in³

@Temperature 77.0 °F
Liquid
1.20 g/cc

@Temperature 25.0 °C
0.0434 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 155 - 185 cP

@Temperature 30.0 °C
155 - 185 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Strength, Yield 63.0 - 68.0 MPa
9140 - 9860 psi
ASTM D638
Elongation at Break 5.0 - 8.0 %
5.0 - 8.0 %
ASTM D638
Tensile Modulus 3.20 - 3.38 GPa
464 - 490 ksi
ASTM D638
Flexural Strength 88.0 - 110 MPa
12800 - 16000 psi
ASTM D790
Flexural Modulus 2.69 - 3.24 GPa
390 - 470 ksi
ASTM D790
Izod Impact, Notched 0.120 - 0.220 J/cm
0.225 - 0.412 ft-lb/in
ASTM D256
Gardner Impact 1.10 J
0.811 ft-lb
ASTM D5420
Penetration 5.2
5.2
mils
Thermal Properties Metric English Comments
CTE, linear 61.0 µm/m-°C

@Temperature 0.000 - 40.0 °C
33.9 µin/in-°F

@Temperature 32.0 - 104 °F
T<Tg; ASTM E831-93
163 µm/m-°C

@Temperature 75.0 - 140 °C
90.6 µin/in-°F

@Temperature 167 - 284 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 58.0 °C
131 - 136 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 53.0 °C
124 - 127 °F
ASTM D648
Glass Transition Temp, Tg 56.0 °C
133 °F
DMA, E"
Descriptive Properties Value Comments
Appearance White
Critical Exposure (mJ/cm²) 7.4
Tested Build Styles FAST™, EXACT™, Exact HR