3M 1400 Economy Vinyl Electrical Tape

Category Polymer , Tape , Thermoplastic , Vinyl (PVC)
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 1400 Economy Vinyl Electrical Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chloride (PVC) backing with pressure-sensitive rubber based adhesive. It inhibits corrosion of electrical conductors.Information provided by 3M
Physical Properties Metric English Comments
Thickness 178 microns
7.00 mil
ASTM D1000
Mechanical Properties Metric English Comments
Elongation at Break 150 %
150 %
ASTM D1000
Peel Strength 0.175 kN/m
1.00 pli
Adhesion to Steel; ASTM D1000
0.175 kN/m
1.00 pli
Adhesion to Backing; ASTM D1000
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Electrical Properties Metric English Comments
Dielectric Strength 35.4 kV/mm
900 kV/in
High Humidity; ASTM D1000
39.4 kV/mm
1000 kV/in
Standard Condition; ASTM D1000
Descriptive Properties Value Comments
Appearance Black