3M 1450 General Purpose Aluminum Foil Tape

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 1450 General Purpose Aluminum Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High tack adhesive for good, instant adhesion to many surfaces.Information provided by 3M
Physical Properties Metric English Comments
Thickness 48.3 microns
1.90 mil
Backing; ASTM D3652
78.7 microns
3.10 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.6 MPa
6180 psi
ASTM D3759
Peel Strength 1.249 kN/m
7.125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Adhesive Type Rubber