3M 1675 Polyester Protective Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 1675 Polyester Protective Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Polyester Protection Tape 1675 is a polyester tape with a low-tack adhesive system for temporary surface protection.Information provided by 3M
Physical Properties Metric English Comments
Thickness 33.0 microns
1.30 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM D3759
Elongation at Break 88 %
88 %
ASTM D3759
Peel Strength 0.0219 kN/m
0.125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Clear