3M 3311 General Purpose Aluminum Foil Tape

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3311 General Purpose Aluminum Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ul 723 listedInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3652
91.4 microns
3.60 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.2 MPa
4670 psi
ASTM D3759
Peel Strength 0.9861 kN/m
5.625 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -23.0 °C
-9.40 °F
Descriptive Properties Value Comments
Adhesive Type Rubber