3M 3325 Copper Foil Tape

Category Metal , Nonferrous Metal , Copper Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3325 Copper Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI/RFI shielding. UL 510 Recognized.Information provided by 3M
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Backing; ASTM D3652
76.2 microns
3.00 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.6 MPa
9370 psi
ASTM D3759
Peel Strength 0.438 kN/m
2.50 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic