3M 396 Super Bond Film

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 396 Super Bond Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Super Bond Film Tape 396 is a polyester film tape for adhering to polyesters, polyethylenes and many other difficult-to-adhere-to surfaces.Information provided by 3M
Physical Properties Metric English Comments
Thickness 43.2 microns
1.70 mil
Backing; ASTM D3752
104 microns
4.10 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.3 MPa
10900 psi
ASTM D3759
Elongation at Break 140 %
140 %
ASTM D3759
Peel Strength 1.53 kN/m
8.75 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F