Material Notes:
3M™ Damping Aluminum Foam Sheet 4014 is an open-cell polyurethane foam with an aluminum constraining layer on one side and a pressure sensitive adhesive on the opposite side to facilitate attachment to the surface of the vibrating panel. The adhesive is protected by an easy-release liner.Information provided by 3M
Thermal Properties Metric English Comments
Thermal Conductivity 0.0690 W/m-K
0.479 BTU-in/hr-ft²-°F
Users viewing this material also viewed the following: