Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 421 Lead Foil Tape

Category Metal , Nonferrous Metal , Lead Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 421 Lead Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Self-wound plating tapeInformation provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
Backing; ASTM D3652
160 microns
6.30 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.4 MPa
2380 psi
ASTM D3759
Peel Strength 0.33964 kN/m
1.9375 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Copyright © lookpolymers.com All Rights Reserved