3M 444PC Double Coated Tapes with Adhesive 300

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 444PC Double Coated Tapes with Adhesive 300.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides relatively high initial adhesion and good shear holding power to a variety of surfaces. The carrier also provides easier handling during slitting and die cutting.Information provided by 3M
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Carrier
35.6 microns
1.40 mil
Backside Adhesive
50.8 microns
2.00 mil
Faceside Adhesive
99.1 microns
3.90 mil
Tape
102 microns
4.00 mil
Liner Caliper
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
to stainless steel, 90°, 15 min RT; ASTM D3330
0.47112 kN/m
2.6875 pli
to Polypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.60259 kN/m
3.4375 pli
to ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.66833 kN/m
3.8125 pli
to stainless steel, 90°, 72 hr RT; ASTM D3330
0.66833 kN/m
3.8125 pli
to Polyester, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.701 kN/m
4.00 pli
to Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.95319 kN/m
5.4375 pli
to stainless steel, 90°, 72 hr at 70°C; ASTM D3330
1.2600 kN/m
7.1875 pli
to stainless steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Long term
121 °C
250 °F
Short term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month