3M 469 Splicing Tapes

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 469 Splicing Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Release Liner
140 microns
5.50 mil
Tape
Mechanical Properties Metric English Comments
Peel Strength 0.657 kN/m
3.75 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 9.00 °C
48.2 °F
Short term
180 °C
356 °F
Long term
Descriptive Properties Value Comments
Adhesive Type 330
Appearance Light Red
Liner 72# Densified Kraft