3M 510 Sandblast Stencil

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 510 Sandblast Stencil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Sandblast Stencil 510, also known as letter perfect, can be used for hand-cut and die-cut applications as a surface protection during blasting procedures.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Liner
1140 microns
45.0 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Peel Strength 0.3287 kN/m
1.875 pli
Adhesion to Granite; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Light green