3M 520ETL Sandblast Stencil

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 520ETL Sandblast Stencil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Sandblast Stencil 520 Series, also known as computer cut, is a tan rubber sandblast stencil featuring three differing liner designs.Information provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
Liner
1140 microns
45.0 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Peel Strength 0.394 kN/m
2.25 pli
Adhesion to Granite; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Gray