3M 5461 Anti-Slip/Anti-Stick Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 5461 Anti-Slip/Anti-Stick Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Anti-Slip/Anti-Stick Tape 5461 has the unique properties of being a premium release surface while also having a high coefficient of friction.Information provided by 3M
Physical Properties Metric English Comments
Thickness 198 microns
7.80 mil
Backing; ASTM D3652
231 microns
9.10 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.2 MPa
9460 psi
ASTM D3759
Elongation at Break 165 %
165 %
ASTM D3759
Peel Strength 0.3287 kN/m
1.875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance White
Liner Silicone coated paper
Users viewing this material also viewed the following: